Figure 5
Polarized (red and green) and non-polarized (blue) NR simulations using a CoTi MRL (red and green) and a high-SLD non-magnetic MRL (blue) with SOI parameters of Λ = 500 Å and σ = 50 Å, i.e. `rough'. (a)–(c) Curves for an SOI SLD of 1, 2 and 3 × 10−6 Å−2, respectively. The high-SLD MRL has an SLD of 8 × 10−6 Å−2 and no magnetic SLD, thus no magnetic splitting. |