view article

Figure 2
Penetration depth D of neutrons as a function of αi/αc. The exemplar curve has been calculated for the cubic chiral magnet Fe0.75Co0.25Si at a neutron wavelength of 5 Å, resulting in a critical angle of αc = 0.37°. Depending on the material species, the absolute values of D and αi/αc will vary and can be determined from equations (1)[link] and (2)[link]. For αi/αc = 1, neutrons begin to undergo small-angle scattering within the bulk volume of the film in the NS-SANS regime. For increasingly larger incident angles, such that αi/αc > 1, the penetration depth of neutrons into the sample is greatly enhanced and NS-SANS measurements can be optimized towards bulk sensitivity in the range of 104 nm below the sample surface.