Figure 5
(a) Post mortem scanning electron micrograph of ZnO NW III after three-point bending testing, demonstrating irreversible deformation. Sequence of the [[5\overline{4}\,\overline{1}2]] Laue spot measured along (b) the left-hand part of the NW and (c) the suspended NW part after nanomechanical testing. Zoom-in of the [[5\overline{4}\,\overline{1}2]] Laue spot measured (d) in the embedded part of the NW and (e) in the suspended NW part, showing a splitting and a streaking of the diffraction peak, respectively. The circles indicate simulated Laue spots considering a rotation of the NW around the [0001] axis. In the case of the split Laue spot, a rotation of 0.20° reproduces the splitting well.