Figure 3
Photographs of the 3D-printed measurement chamber, (a)–(c) from different angles, (d) from the top including the neutron (white) and laser light (blue) pathways, (e) from diagonally above, where the neutron exit window is visible, and (f) of the sample holder with an Si wafer fixed to a thin plastic plate. For simultaneous QENS and Raman measurements, the plastic plate was replaced by an aluminium plate to minimize the scattering background. The PEDOT:PSS film on the Si substrate was fixed to this aluminium plate by means of aluminium wire. |