Figure 8
Coupled lattice and shape deformations. Modelling of powder-scattering data from powders of Pd nanocrystals along the Bain (1924 ) deformation path (unit cell 0.389070 nm, size 10 nm). (A) F.c.c. nanocube deforms to the metastable body-centred tetragonal (b.c.t.10) structure through the body-centred cubic (b.c.c.) end member. (B) Scattering intensity profiles modelled using the WPDFM method and lattice deformation matrix only (lines) are compared with the average solution of the Debye scattering equation for a set of 100 equivalent crystals with random position of the shape relative to the lattice (dots). (C) Scattering intensity profiles modelled using the WPDFM method and both lattice and shape deformation tensors (lines) are compared with the average solution of the Debye scattering equation for a set of 100 equivalent crystals with random position of the shape relative to the lattice (dots). The independent global optimization of the Debye profiles modelled with the WPDFM from an f.c.c. 8 nm cubic crystal yielded the estimation of the true parameters with an error of <0.5% and goodness of fit of <0.01. |