Figure 6
Changes in average crystallite size (solid squares) and dislocation density (open circles) for the LiF20h sample during non-isothermal in situ X-ray diffraction at a 10 K min−1 heating rate. |
|
Figure 6
Changes in average crystallite size (solid squares) and dislocation density (open circles) for the LiF20h sample during non-isothermal in situ X-ray diffraction at a 10 K min−1 heating rate. |