view article

Figure 4
(a) Auger map of the surface elemental composition of the sample with 70 nm thickness of Al2O3 after 9 h irradiation in He atmosphere at 1.3 mbar pressure. The same region is represented via SEM (b). Both exposed and unexposed regions were observed (marked on the SEM image).