Figure 6
Typical P(h) diagrams observed during the nanoindentation measurements of beryllium substrate and beryllium substrate coated with ALD alumina of different thicknesses at maximum applied load Pmax = 10 mN (a) and Pmax = 800 µN (b). |
|