Micro-roughness values of an uncoated super-polished silicon substrate (A) and two Pt-coatings with a thickness of 32 nm (B) and 102 nm (C). The values were measured at three positions on each sample using white-light interferometry with magnifications of 20× (left) and 50× (right).