Figure 5
Time histories of temperature at three different distance r = 0, 20, 50 µm on the front surface (z = 0, solid) and back surface (z = 40 µm, dashed) in a 40 µm-thick diamond plate upon a single-pulse laser of 20 µm waist-size. |
|
Figure 5
Time histories of temperature at three different distance r = 0, 20, 50 µm on the front surface (z = 0, solid) and back surface (z = 40 µm, dashed) in a 40 µm-thick diamond plate upon a single-pulse laser of 20 µm waist-size. |