Figure 3
Data extracted from a series of images recorded during the experiment shown in Fig. 2. (a) The total intensity of the superstructure rod from the ()-R27° surface oxide plotted together with the CO2 PLIF signal extracted from the blue rectangle indicated in the PLIF images in Fig. 2, allowing for a better correlation between the surface structure and CO2 production. (b) The same PLIF CO2 signal as in (a) plotted together with the CO2 MS signal. |