The pressure dependence of the magnetic diffraction peaks of Sr3Ir2O7 measured by collecting the elastic signal while scanning along the high-symmetry directions of the reciprocal lattice parallel to (a) the (100) axis and (b) the (001) axis. The scans were collected at T = 100 K. |