research papers
A compact furnace for in situ X-ray absorption spectroscopy: design, fabrication and study of cationic oxidation states in Pr6O11 and NiO
aSynchrotron Light Research Institute, Nakhon Ratchasima 30000, Thailand, bSchool of Physics, Institute of Science, Suranaree University of Technology, Nakhon Ratchasima 30000, Thailand, and cResearch Network NANOTEC-SUT on Advanced Nanomaterials and Characterization, School of Physics, Institute of Science, Suranaree University of Technology, Nakhon Ratchasima 30000, Thailand
*Correspondence e-mail: suchinda@slri.or.th
A well designed compact furnace has been designed for in situ It enables various heat ramps from 300 K to 1473 K. The furnace consists of heaters, a quartz tube, a circulated refrigerator and a power controller. It can generate ohmic heating via an induction process with tantalum filaments. The maximum heating rate exceeds 20 K min−1. A quartz tube with gas feedthroughs allows the mixing of gases and adjustment of the flow rate. The use of this compact furnace allows in situ investigations to be carried out in transmission or fluorescence modes under controlled temperature and atmosphere. Moreover, the furnace is compact, light and well compatible to The furnace was used to study cationic oxidation states in Pr6O11 and NiO compounds under elevated temperature and reduced atmosphere using the in situ X-ray absorption near-edge structure (XANES) technique at beamline 5.2 SUT-NANOTEC-SLRI of the Synchrotron Light Research Institute, Thailand. At room temperature, Pr6O11 contains a mixture of Pr3+ and Pr4+ cations, resulting in an average of +3.67. In situ XANES spectra of Pr (L3-edge) show that the of Pr4+ cations was totally reduced to +3.00 at 1273 K under H2 atmosphere. Considering NiO, Ni2+ species were present under ambient conditions. At 573 K, the reduction process of Ni2+ occurred. The Ni0/Ni2+ ratio increased linearly with respect to the heating temperature. Finally, the reduction process of Ni2+ was completely finished at 770 K.
Keywords: X-ray absorption spectroscopy; in situ cells; transmittance and fluorescence; instrumentations; in situ XAFS.
1. Introduction
et al., 2019; Song et al., 2019; Jaiban et al., 2018; Sumrunronnasak et al., 2018; Sriplai et al., 2018; Boonruang et al., 2018). It is well known that the performance of the technique can be enhanced by utilizing in situ cells which enable experimental conditions, such as elevated temperature, vacuum, inert and reducing/oxidizing atmosphere, to be controlled in real time. According to the literature, in situ heating cells have been developed using different approaches for time- or temperature-resolved techniques (Tamura et al., 1995; Lamberti et al., 2003; Huwe & Fröba, 2004; Meneses et al., 2006; An et al., 2014; Yamamoto et al., 2018; Zhao et al., 2017; Inukai et al., 2015). Most were initially fabricated for the purpose of investigations on catalyst materials (van Bokhoven et al., 1999; van der Eerden et al., 2000; Grunwaldt et al., 2001; Kappen et al., 2001; Bolin et al., 2013; Yamamoto et al., 2018; Mathisen et al., 2018). Recently, the in situ technique has also been applied to characterize other advanced and novel materials (Steiner et al., 2019; Deb et al., 2006; Hashimoto et al., 2007; Massa et al., 2015; Marini et al., 2018; Mastelaro et al., 2018; Chin et al., 2019). Nevertheless, these in situ heating cells possess some limitations in terms of maximum temperature, heating rate, flowing gas or measurement mode. Therefore, it has been interesting to design an in situ furnace with optimized functionalities and qualities.
performed at synchrotron sources has been considered a powerful characterization tool for several decades due to its high sensitivity and its capability to probe almost all elements of the periodic table. This technique is non-destructive and is suitable for studying a large variety of materials such as powders, solids, liquids, glasses, thin films, crystals and amorphous compounds. Basically, spectra consist of X-ray absorption near-edge structure (XANES) and extended X-ray absorption fine structure (EXAFS). The spectra can be used to determine the cationic/anionic chemical geometry, oxygen vacancy and local structure of a probed element. Therefore, it is frequently used to sustainably develop physical, thermo-electric, catalytic or magnetic properties of advanced and novel materials (YaoIn this work, we demonstrate the design, thermal simulation, fabrication and performance tests for an in situ furnace. The compact furnace was designed simply using inexpensive materials. The sample holder is designed to be adaptable for in situ transmission and fluorescence measurements. The furnace can be easily installed at synchrotron facilities and combined with gas lines. To the best of our knowledge, the compact in situ furnace possesses superior specifications to the previously mentioned in situ heating cells in terms of maximum temperature, heating rate and capability to perform measurements in both transmission and fluorescence modes. In addition, the furnace atmosphere can be controlled by pumping under vacuum or flowing any type of gas such as H2, N2, O2, Ar, He or CO2 with an adjustable rate between 1 and 100 ml min−1. Finally, we tested the quality and performance of the fabricated compact furnace at beamline 5.2 SUT-NANOTEC-SLRI at the Synchrotron Light Research Institute (SLRI), Nakhon Ratchasima, Thailand, which is capable of tuning X-ray energy from 1.2 keV to 13.0 keV. In situ experiments were operated from 300 K to 1473 K under H2 atmosphere. The XANES experiments were performed by probing Pr and Ni elements at the L3-edge and K-edge in transmission and fluorescence modes, respectively. The obtained spectra were normalized using Athena software (Ravel & Newville, 2005). A linear combination fit was also performed to investigate changes in the oxidation states and weight percentages of cationic ions in Pr6O11 and NiO compounds.
Based on conventional
measurements in the tender X-ray range at beamline 5.2, SLRI, such a probing Si, Mg or Al XANES/EXAFS experiment could be performed by using double single-crystals of beryl () as a monochromator and sealing the photon-in and photon-out windows with polypropylene tape. Note that a flowing He atmosphere is necessary to obtain a good signal.2. In situ compact furnace
The compact furnace was designed and developed to achieve high performances and optimal functionalities for in situ measurement. The furnace system consists of four main components. First, a compact furnace equipped with a thermocouple and a proportional integral derivative (PID) controller. The PID controller has a set of digital temperature programs, including two patterns; the maximum number of steps is 16. Second, a three-way quartz tube, used as the sample holder. Third, flanged windows, enclosing the quartz tube for the photon-in pathway A and the photon-out pathways B and C. The windows are sealed by Kapton (polyimide) tape of thickness 50 µm. Kapton can be replaced by another window material such as polypropylene or beryllium, depending on the X-ray energy range. Furthermore, the feedthroughs of the gas inlet and outlet, mounted at the flange windows, allow the distribution of various types of gas such as H2, N2, He, Ar, CO2 and O2 into the quartz tube. The flow rate can be adjusted from 1 to 100 ml min−1 with gas mass flow controllers. Fourth, a cooling chamber, connected to a water-circulated refrigerator. It should be noted that flowing He gas is suggested during measurements at photon energies below 3000 eV in fluorescence mode to improve the signal-to-noise ratio; above 3000 eV, experiments can be performed under air. Fig. 1 shows the construction drawing of the entire compact furnace; specifications of the compact furnace are summarized in Table 1. The main components of the in situ furnace are depicted and detailed in Fig. 2 and Table 2, respectively.
|
|
A thermal simulation was also conducted for the entire area of the furnace using SolidWorks (https://www.solidworks.com/) software as shown in Fig. 1 (inset). The heating zone was uniformly distributed and covered all of the furnace's body, precisely in an area of 100 mm × 100 mm. With these specifications, the maximum temperature can exceed 1473 K. The heating rate can be varied between 1 and 20 K min−1. The furnace is equipped with a PID controller, enabling 16 heating steps to be programmed. Moreover, a sample holder was specially designed to be adaptable for measuring in situ in transmission and fluorescence modes. Hence, the ceramic holder was cut and mounted at angles of 45° and 90°. Here, the sample holder can be put inside the three-ways quartz tube and placed together in the middle of the furnace.
Regarding Fig. 1, the monochromatic X-ray beam enters via entrance A and reaches the sample at the furnace center. In the case of transmission mode, the X-ray beam penetrates the sample and passes through the via pathway B. On the other hand, fluorescence emission can occur and is measured by using a solid-state detector at the end of pathway C. Here, we used a silicon drift detector (SDD), which is extremely sensitive to elevated temperature. Therefore, we fabricated a cooling chamber to prevent heat damage during in situ measurement. It was inserted between the heating zone and the SDD (see `5' in Fig. 1). This chamber has a window flange at the end, equipped with a high-performance refrigerated circulator (JULABO, model Corio CD-200F). The maximum cooling temperature was 178 K.
In order to test its quality and heating performance, all of the main components were systematically connected and installed at beamline 5.2 SUT-NANOTEC-SLRI shows a photograph of the in situ system showing its configuration.
at SLRI. Fig. 3The functionalities of the compact furnace were tested by recording the measured temperature inside the furnace under N2 atmosphere at a flow rate of 10 ml min−1. The heating temperature was ramped from room temperature to 1473 K with different heating rates of 2, 5, 10 and 20 K min−1. Once the maximum temperature was reached, the furnace was held at 1473 K for at least 30 min to observe any thermal fluctuation. For all heating rates, the measured and set temperatures were well superposed, as shown in Fig. 4. Fig. 4 shows that the invented furnace achieved heating from room temperature to a maximum temperature of 1200 K with no thermal fluctuation during the tests at heating rates of 2, 5, 10 and 20 K min−1.
3. X-ray absorption spectroscopy
After furnace testing, in situ experiments were carried out in order to study the reduction process of cationic ions in Pr6O11 and NiO fine powders in transmission and fluorescence modes, respectively. In this section, we determine the effect of temperature on cationic in Pr6O11 and NiO compounds. Fine powders were ground and compressed into pellets of diameter 15 mm. Our furnace was set up and in situ experiments were performed at beamline 5.2 to record the Pr and Ni XANES in transmission and fluorescence modes, respectively. The stored current was around 120 mA. Germanium (220) double single-crystals were utilized as a monochromator to probe the Pr and Ni elements at their L3-edge (5964 eV) and K-edge (8333 eV), respectively. The data interval was set as 0.3 eV. The measurements were carried out at various temperatures ranging from 300 to 1473 K under H2 reducing atmosphere. Using Athena software, the recorded XANES spectra were normalized and interpreted to study the changes in the oxidation states for Pr and Ni cations.
3.1. Pr L3-edge XANES
Pr6O11 commercial powder was compressed into a pellet of diameter 15 mm and placed at an angle of 90° in the sample holder. Heating steps were programed from room temperature to 1473 K with a heating rate of 10 K min−1. Firstly, measurements were made in transmission mode by probing Pr at its L3 at 5964 eV. The photon energy was tuned using the Ge (220) double-crystal monochromator. In situ XANES spectra were collected during heating the sample under H2 atmosphere with a flow rate of 20 ml min−1. Fig. 5 shows all the normalized spectra at various temperatures.
Consider a mixture of Pr3+ and Pr4+ cations in Pr6O11 compound at ambient atmosphere. According to charge neutralization, the corresponding weight percentages are derived to be 33.3% and 66.7%, respectively. This resulted in an average of +3.67. Based on the recorded XANES spectra, the corresponding was located at a photon energy of 5968.1 eV. Main peaks at 5970.4 eV and 5981.2 eV contributed to 4f2 and 4f1 electronic configurations, respectively (Ogier et al., 2019). As the temperature reaches 470 K, the shifts significantly towards lower energy. This indicates the reduction of Pr ions: Pr4+ ions were partially reduced to Pr3+ ions. As a result, the intense peak of Pr4+ species at 5981.5 eV decreased as a function of temperature. This can be attributed to the increasing ratio of Pr3+/Pr4+. Furthermore, the white line peak of Pr4+ species at 5981.2 eV was absent when the reduction process was completely finished at 1273 K. This is in good accordance with the work of Luo et al. (2006), which reported that Pr6O11 was reduced at high temperature and completely transformed to Pr2O3 around that temperature.
Moreover, we determined the weight percentage of the crystalline phases of Pr6O11 and Pr2O3 during reduction under H2 atmosphere by processing a linear combination fit (LCF) for the energy range −30 to 30 eV from the Pr L3 The fit results are demonstrated in Table 3, and suggest that R-factors of all fitting results are below 0.015, indicating high accuracy and reliability of the LCF fitting.
|
3.2. Ni K-edge XANES
NiO commercial powders were mixed with boron nitride powders in order to dilute the Ni content and compressed into pellets. A pellet was placed in the sample holder at an angle of 45° and loaded together into the center of the furnace for in situ fluorescence operation. XANES measurements were carried out by probing Ni at 8333 eV. The in situ beamline configuration was set up as previously described in Section 3.1. Here, the SDD detector was utilized for measuring the signal. The water cooling temperature was set at 283 K to prevent heat damage to the SDD. The heating steps were programmed from room temperature to 773 K to investigate the reduction process of Ni2+ ions in NiO compounds under H2 flowing gas with a heating rate of 20 ml min−1. Also, XANES spectra of Ni foil and NiO compound with were recorded under ambient conditions and used as references for Ni0 and Ni2+ species. The results are shown in Fig. 6.
Fig. 6 shows absorption edges at 8333.3 eV and 8344.4 eV for Ni foil and NiO, respectively. As a result, these characteristic values can be used as references for Ni0 and Ni2+ species.
Considering the Ni K-edge XANES spectra of NiO compound recorded at various temperatures (see Fig. 7), its obviously decreased from 620 K. It is noteworthy that the intensity of the white line peak at 8351 eV, generated by scattering between central Ni atoms and surrounding O atoms, also declined. This suggests that Ni2+ ions were partially reduced to Ni0 metallic species with increasing temperature. The spectrum recorded at 770 K is similar to that of the Ni foil. As shown in Table 4, the reduction process was completely finished at 770 K.
|
4. Conclusions
The design, fabrication and performance of a compact furnace for in situ heating experiments have been described. The furnace can be easily installed at synchrotron facilities for measurements in transmission and fluorescence modes from 300 to 1473 K with no heating fluctuation. The maximum heating rate exceeds 20 K min−1. The experimental atmosphere can be controlled by flowing or mixing gas with an adjustable flow rate from 1 to 100 ml min−1. The furnace was successfully set up at beamline 5.2 (SLRI, Thailand) for in situ operation. Transmission XANES spectra at various temperatures indicated the reduction of Pr ions in Pr6O11 catalyst compounds under H2 reducing atmosphere (average from +3.67 to +3) and the Pr6O11 → Pr2O3 at 1173 K. Further, in situ spectra of Ni in fluorescence mode showed the reduction of Ni2+ ions to Ni0 metallic species at 620 K. Therefore, our furnace is very suitable for investigation of temperature-dependent structure transitions such as metallic melts, nanoparticles phase-change and the solidification process of crystalline materials.
Funding information
Funding and the well equipped machine shop were supported by the Synchrotron Light Research Institute (SLRI) in Thailand. This work has been partially supported by the Research Network NANOTEC (RNN) program of the National Nanotechnology Center (NANOTEC), National Science and Technology Development Agency (NSTDA), Ministry of Higher Education, Science, Research and Innovation (MHESI), Thailand.
References
An, P., Hong, C., Zhang, J., Xu, W. & Hu, T. (2014). J. Synchrotron Rad. 21, 165–169. Web of Science CrossRef CAS IUCr Journals Google Scholar
Bokhoven, J. A. van, van der Eerden, A. M. J., Smith, A. D. & Koningsberger, D. C. (1999). J. Synchrotron Rad. 6, 201–203. Web of Science CrossRef IUCr Journals Google Scholar
Bolin, T. B., Wu, T., Schweitzer, N., Lobo-Lapidus, R., Kropf, A. J., Wang, H., Hu, Y., Miller, J. T. & Heald, S. M. (2013). Catal. Today, 205, 141–147. Web of Science CrossRef CAS Google Scholar
Boonruang, C., Thong-on, A. & Kidkhunthod, P. (2018). Sci Rep, 8, 2289. Web of Science CrossRef PubMed Google Scholar
Chin, Y. Y., Lin, H., Hu, Z., Shimakawa, Y. & Chen, C. (2019). Physica B, 568, 92–95. Web of Science CrossRef CAS Google Scholar
Deb, A., Ralph, J. M., Cairns, E. J. & Bergmann, U. (2006). Phys. Rev. B, 73, 115114. Web of Science CrossRef Google Scholar
Eerden, A. M. J. van der, van Bokhoven, J. A., Smith, A. D. & Koningsberger, D. C. (2000). Rev. Sci. Instrum. 71, 3260–3266. Web of Science CrossRef Google Scholar
Grunwaldt, J.-D., Kappen, P., Hammershøi, B. S., Tröger, L. & Clausen, B. S. (2001). J. Synchrotron Rad. 8, 572–574. Web of Science CrossRef CAS IUCr Journals Google Scholar
Hashimoto, T., Yoshiasa, A., Okube, M., Okudera, H. & Nakatsuka, A. (2007). AIP Conf. Proc. 882, 428–430. CrossRef CAS Google Scholar
Huwe, H. & Fröba, M. (2004). J. Synchrotron Rad. 11, 363–365. Web of Science CrossRef CAS IUCr Journals Google Scholar
Inukai, K., Iwai, H., Takahashi, Y. & Shin, W. (2015). Ceram. Int. 41, 2852–2862. Web of Science CrossRef CAS Google Scholar
Jaiban, P., Watcharapasorn, A., Yimnirun, R., Guo, R. & Bhalla, A. S. (2018). J. Alloys Compd. 759, 120–127. Web of Science CrossRef CAS Google Scholar
Kappen, P., Grunwaldt, J., Hammershøi, B. S., Tröger, L. & Clausen, B. S. (2001). J. Catal. 198, 56–65. Web of Science CrossRef CAS Google Scholar
Lamberti, C., Prestipino, C., Bordiga, S., Berlier, G., Spoto, G., Zecchina, A., Laloni, A., La Manna, F., D'Anca, F., Felici, R., D'Acapito, F. & Roy, P. (2003). Nucl. Instrum. Methods Phys. Res. B, 200, 196–201. Web of Science CrossRef CAS Google Scholar
Luo, M.., Yan, Z.. & Jin, L.. (2006). J. Mol. Catal. A, 260, 157–162. Web of Science CrossRef CAS Google Scholar
Marini, C., Diaz-Rovira, A. M., Kennedy, B. J. & Joseph, B. (2018). J. Mater. Eng. Perform. 27, 6322–6327. Web of Science CrossRef CAS Google Scholar
Massa, N. E., Ramos, A. Y., Tolentino, H. C. N., Sousa-Neto, N. M., Fonseca, J. Jr & Alonso, J. A. (2015). Mater. Res. Expr. 2, 126301. Web of Science CrossRef Google Scholar
Mastelaro, V. & Zanotto, E. (2018). Materials (Basel), 11, 204. Web of Science CrossRef Google Scholar
Mathisen, K., Kirste, K. G., Hargreaves, J. S. J., Laassiri, S., McAulay, K., McFarlane, A. R. & Spencer, N. A. (2018). Top. Catal. 61, 225–239. Web of Science CrossRef CAS PubMed Google Scholar
Meneses, C. T., Flores, W. H., Sotero, A. P., Tamura, E., Garcia, F. & Sasaki, J. M. (2006). J. Synchrotron Rad. 13, 468–470. Web of Science CrossRef CAS IUCr Journals Google Scholar
Ogier, T., Prestipino, C., Figueroa, S., Mauvy, F., Mougin, J., Grenier, J. C., Demourgues, A. & Bassat, J. M. (2019). Chem. Phys. Lett. 727, 116–120. Web of Science CrossRef CAS Google Scholar
Ravel, B. & Newville, M. (2005). J. Synchrotron Rad. 12, 537–541. Web of Science CrossRef CAS IUCr Journals Google Scholar
Song, T., Yao, W., Kiadkhunthod, P., Zheng, Y., Wu, N., Zhou, X., Tunmee, S., Sattayaporn, S. & Tang, Y. (2020). Angew. Chem. Int. Ed. 59, 740–745. Web of Science CrossRef CAS Google Scholar
Sriplai, N., Koowattanasuchat, S., Kidkhunthod, P., Chanlek, N., Eichhorn, S. J. & Pinitsoontorn, S. (2018). J. Alloys Compd. 739, 19–29. Web of Science CrossRef CAS Google Scholar
Steiner, C., Gänzler, A. M., Zehentbauer, M., Hagen, G., Casapu, M., Müller, S., Grunwaldt, J. & Moos, R. (2019). Top. Catal. 62, 227–236. Web of Science CrossRef CAS Google Scholar
Sumrunronnasak, S., Chanlek, N. & Pimpha, N. (2018). Mater. Chem. Phys. 216, 143–152. Web of Science CrossRef CAS Google Scholar
Tamura, K., Inui, M. & Hosokawa, S. (1995). Rev. Sci. Instrum. 66, 1382–1384. CrossRef CAS Web of Science Google Scholar
Yamamoto, Y., Suzuki, A., Tsutsumi, N., Katagiri, M., Yamashita, S., Niwa, Y., Katayama, M. & Inada, Y. (2018). J. Solid State Chem. 258, 264–270. Web of Science CrossRef CAS Google Scholar
Yao, W., Armstrong, A. R., Zhou, X., Sougrati, M. T., Kidkhunthod, P., Tunmee, S., Sun, C., Sattayaporn, S., Lightfoot, P., Ji, B., Jiang, C., Wu, N., Tang, Y. & Cheng, H. M. (2019). Nat. Commun. 10, 3483. Web of Science CSD CrossRef PubMed Google Scholar
Zhao, N., Yao, M. J., Ma, H. T. & Wong, C. P. (2017). J. Mater. Sci. Mater. Electron. 28, 8824–8831. Web of Science CrossRef CAS Google Scholar
© International Union of Crystallography. Prior permission is not required to reproduce short quotations, tables and figures from this article, provided the original authors and source are cited. For more information, click here.