X-ray images of a test pattern and the corresponding line profiles taken with a 10× objective with NA ≃ 0.45. A 180 µm CdWO4 scintillator with no substrate (left). A 180 µm CdWO4 scintillator with 2 mm LuAG substrate (right). The resolution of the right image is better.