Figure 9
(a) Unit-cell volume (left axis) of ɛ- and γ-Fe and temperature (right axis) as a function of laser power, at 70 GPa. (b) XRD patterns of the sample assembly before heating (black), at temperatures of the first sign of melting (red) and when the iron sample is almost completely molten (green) at temperatures above the melting curve. The inset shows the residual diffuse signal after subtracting the room-temperature pattern.