Figure 13
Early results from the CuCrZr deformation commissioning experiment. (a) Load–displacement curve: elastic deformation occurs up to 200 µm displacement. (b) 3D rendering of plastically deformed CuCrZr; shear bands of voids are present in the necking region in green, highlighted by the green arrow. (c) 2D diffraction pattern. The integration was performed over a 10° angle in the loading direction. (d) Peak shift of the (311) peak indicating the application of strain in the elastically strained state. The peak position stays constant in the plastic region. |