Example of data fitting for a powder antiferromagnetic sample (SmFeAsO) at 5 K under an external magnetic field of 7.9 T oriented perpendicular to the magnetic vector of the beam. Fitting was performed utilizing the model described in Section 3.4.1[link]. The green line is a residual between the experimental spectrum and the model. The cyan line is the difference between a model calculated with a selected number of points per integration and that with four times more points.