Figure 3
Intensity–intensity correlation function measured on Pt42.5Cu27Ni9.5P21 and Au49Cu26.9Si16.3Ag5.5Pd2.3 ribbons at 7 GPa and 2 GPa, respectively, at the P10 beamline of the PETRA III source, and at the ID10 beamline of the ESRF. For both samples, the ribbons were prepared from the same batch, and thinned to the same thickness (around 15 µm).