Comparison of experimental (lines) and model (squares) Zn-doped HAP FT, Zn K-edge, model with Zn inserted in the unit cell of HAP. Taking into account the error bars (drawn at 1[sigma]), the FT is completely reproduced, since the last two small peaks are not significant (from Chassot et al., 2001BB6).  [article HTML]