Figure 2
Change in temperature of samples as a function of incident flux, with 0.19 mm-thick and 0.025 mm-thin Cu wire aligned end-on or side-on to the beam, a 0.5 mm capillary of CeO2, and 0.5 mm Al wire. |
Open
access

|
Figure 2
Change in temperature of samples as a function of incident flux, with 0.19 mm-thick and 0.025 mm-thin Cu wire aligned end-on or side-on to the beam, a 0.5 mm capillary of CeO2, and 0.5 mm Al wire. |