Figure 11
(a) Scanning electron microscopy (SEM) images of a fractured CePd2Si2 polycrystalline sample. (b) Intensity plot of Ce 3d resonant HAXPES spectra at the Ce L3 edge. (c) Ce 3d HAXPES spectrum at a non-resonant condition (hν = 5.712 keV). (d) Constant initial state spectra for 3d3/2f0 (binding energy, EB = 913.8 eV), 3d5/2f1 (EB = 882.7 eV) and 3d5/2f2 peaks (EB = 877.3 eV). |